Compenent | Appearance | Size | Bulk Density(kg/l) | BET | Pore Volume(ml/g) | Crushing Strength(N/Particle) | Na2O % | Al2O3 % | Water absorption |
Al2O3·nH2O | Round bar | 3*(4-10) | 0.55-0.65 | ≥ 150 | ≥ 0.50 | ≥ 100 | ≤0.10 | ≥ 94 | ≥ 70 |
Al2O3·nH2O | Trilobe | 3*(4-10) | 0.55-0.65 | ≥ 150 | ≥ 0.50 | ≥ 100 | ≤0.10 | ≥ 94 | ≥ 70 |
Al2O3·nH2O | Round bar | 3*(4-10) | 0.5-0.6 | ≥ 220 | ≥ 0.60 | ≥ 90 | ≤0.10 | ≥ 94 | ≥ 70 |
Al2O3·nH2O | Trilobe | 3*(4-10) | 0.5-0.6 | ≥ 220 | ≥ 0.60 | ≥ 90 | ≤0.10 | ≥ 94 | ≥ 70 |
Si Al composite | Round bar | 3*(4-10) | 0.5-0.6 | ≥ 180 | ≥ 0.50 | ≥ 100 | ≤0.10 | ≥ 84 | ≥ 65 |
Si Al composite | Trilobe | 3*(4-10) | 0.5-0.6 | ≥ 180 | ≥ 0.50 | ≥ 100 | ≤0.10 | ≥ 84 | ≥ 65 |
Ti Al composite | Round bar | 3*(4-10) | 0.55-0.65 | ≥ 150 | ≥ 0.45 | ≥ 90 | ≤0.15 | ≥ 84 | ≥ 72 |
Ti Al composite | Trilobe | 3*(4-10) | 0.55-0.65 | ≥ 150 | ≥ 0.45 | ≥ 90 | ≤0.15 | ≥ 84 | ≥ 72 |
Al2O3·nH2O | Round bar | 3*(4-10) | 0.70-0.80 | ≥ 180 | ≥ 0.40 | ≥ 80 | ≤0.10 | ≥ 94 | ≥ 50 |
Al2O3·nH2O | Ball | Φ3-4 | ≥ 0.68 | ≥ 170 | ≥ 0.45 | ≥ 70 | ≤0.20 | ≥ 94 | ≥ 65 |
Al2O3·nH2O | Ball | Φ5-7 | ≥ 0.68 | ≥ 170 | ≥ 0.45 | ≥ 130 | ≤0.25 | ≥ 94 | ≥ 50 |
Al2O3·nH2O | Ball | Φ4-6 | 0.55-0.60 | ≥ 250 | ≥ 0.45 | ≥ 60 | 0.10-1.00 | ≥ 94 | ≥ 60-70 |
Al2O3·nH2O | Trilobe | 3*(4-10) | 0.45-0.60 | ≥ 350 | ≥ 0.65 | ≥ 70 | ≤0.10 | ≥ 95 | ≥ 80 |